elobau

SEKO magnet 340004


340004 Product inquiry
temperature coefficient -0,042%/K -0,03%/K (SmCo5/Sm2Co17), -0,12%/K (NdFeB)
temperature range -40C +250C (SmCo5), -40C +350C (Sm2Co17), -40C +130C (NdFeB)
Curie temperature 720C (SmCo5), 825C (Sm2Co17), 330C (NdFeB)
Br typ. 880-1010 mT (SmCo5/Sm2Co17), typ. 1170 - 1240 mT (NdFeB)
HcB typ. 690-730 kA/m (SmCo5/Sm2Co17), typ. 870-940 kA/m (NdFeB)
HcJ typ. 2000 kA/m (SmCo5/Sm2Co17), typ. 1360 kA/m (NdFeB)
BH max typ. 155-200 kJ/m3 (SmCo5/Sm2Co17), typ. 255-300 kJ/m3 (NdFeB)
orientation anisotropic
hardness 6-7 Mohs (SmCo5/Sm2Co17), HV 10: 560-580 (NdFeB)
Contact Sweden
We use cookies for analysis and marketing purposes. By continuing to use this website, you agree to the use of cookies. Further information can be found in our data privacy policy. Please press the OK button if you want to view our policy. You can prevent cookies from being stored by adjusting your browser settings.