temperature coefficient -0,042%/K -0,03%/K (SmCo5/Sm2Co17), -0,12%/K (NdFeB)
temperature range -40C +250C (SmCo5), -40C +350C (Sm2Co17), -40C +130 C (NdFeB)
Curie temperature 720C (SmCo5), 825C (Sm2Co17), 330C (NdFeB)
Br typ. 880-1010 mT (SmCo5/Sm2Co17), typ. 1170 - 1240 mT (NdFeB)
HcB typ. 690-730 kA/m (SmCo5/Sm2Co17), typ. 870-940 kA/m (NdFeB)
HcJ typ. 2000 kA/m (SmCo5/Sm2Co17), typ. 1360 kA/m (NdFeB)
BH max typ. 155-200 kJ/m3 (SmCo5/Sm2Co17), typ. 255-300 kJ/m3 (NdFeB)
orientation anisotropic
hardness 6-7 Mohs (SmCo5/Sm2Co17), HV 10: 560-580 (NdFeB)